ABSTRACT:
A composite refractory material is prepared by combining boron carbide with furan resin to form a mixture containing about 8 wt. % furan resin. The mixture is formed into a pellet which is placed into a grit pack comprising an oxide of an element such as yttrium to form a sinterable body. The sinterable body is sintered under vacuum with microwave energy at a temperature no greater than 2000.degree. C. to form a composite refractory material.

REFERENCES:
patent: 5164130 (1992-11-01), Holcombe et al.
patent: 5321223 (1994-06-01), Kimrey, Jr. et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of making a composite refractory material does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of making a composite refractory material, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making a composite refractory material will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1550680

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.