Method of increasing yield of petroleum pitch

Mineral oils: processes and products – Asphalts – tars – pitches and resins; making – treating and... – Chemical modification of asphalt – tar – pitch or resin

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C10G 3706

Patent

active

042435137

ABSTRACT:
Clarified slurry oil feedstock is heated at temperatures above 340.degree. C. and preferably between 390.degree. C. and 410.degree. C. for periods exceeding a minimum of about 2 hours, under reflux conditions and in the absence of air, so as to maximize the polymerization of light ends in the formation of petroleum pitch. An increased yield of petroleum pitch is obtained from the clarified slurry oil feedstock.

REFERENCES:
patent: 2992181 (1961-07-01), Renner
patent: 3288701 (1966-11-01), Fauber et al.
patent: 3318801 (1967-05-01), Alexander et al.
patent: 3355377 (1967-11-01), King
patent: 4017378 (1977-04-01), Fauveau et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of increasing yield of petroleum pitch does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of increasing yield of petroleum pitch, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of increasing yield of petroleum pitch will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-283866

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.