ABSTRACT:
Pig iron is refined by top blowing with oxygen and injecting inert gas from the bottom. The slag formation is minimized by controlled addition of lime to match the formation of slag components as they are generated by the process. This increases the capacity of the melt to receive a cold charge, e.g. of scrap.

REFERENCES:
patent: 3854932 (1974-12-01), Bishop
patent: 4329171 (1982-05-01), Robert
patent: 4365992 (1982-12-01), Sieckman
Article in Iron and Steel Engineer, 58, No. 12, Dec. 1981, pp. 34-38, by Francis Schleimer et al. "Development of the LBE Process."

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of increasing the cold material charging capacity in the does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of increasing the cold material charging capacity in the , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of increasing the cold material charging capacity in the will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1753682

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.