ABSTRACT:
A process is described in which an iron-silicon alloy capable of being heat treated to produce a cube-on-edge (110) [001] grain orientation is treated to produce improved core losses when the material is under high operating inductions. The process steps include cleaning the surface of the steel of finish gauge thickness, applying a coating to the surface of the steel which is non-reactive with the surface and promotes decarburization, heating to a temperature sufficiently high to effect secondary recrystallization texture development and decarburization and cooling to room temperature. Data are included which demonstrate the improved core losses exhibited by these materials so treated when tested at high operating inductions.
REFERENCES:
patent: 3116179 (1963-12-01), Carpenter et al.
patent: 3159511 (1964-12-01), Taguchi et al.
patent: 3333993 (1967-08-01), Kohler
patent: 3523837 (1970-08-01), Pavlik
patent: 3528863 (1970-09-01), Foster et al.
patent: 3615903 (1971-10-01), Perry et al.
patent: 3676227 (1972-07-01), Matsumoto et al.
patent: 3700506 (1972-10-01), Tanaka et al.
patent: 3785882 (1974-01-01), Jackson
Randig R. T.
Satterfield Walter R.
Westinghouse Electric Corporation
LandOfFree
Method of improving the core-loss characteristics of cube-on-edg does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of improving the core-loss characteristics of cube-on-edg, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of improving the core-loss characteristics of cube-on-edg will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-744952