ABSTRACT:
A method of heat treatment for an efficient forming of two-layered oxide film on the inside surface of a Ni-base alloy tube. The oxide film suppresses the Ni release in a high-temperature water environment.At least two gas supplying devices are provided on the outlet side of a continuous heat treatment furnace; or one gas supplying device is provided respectively on the outlet side and the inlet side thereof. The tube is put into the furnace while supplying an atmospheric gas into the tube from the front end of the tube moving direction with one of these gas supplying devices and a gas introducing pipe, which is arranged inside the furnace, and this tube is maintained at 650 to 1200° C. for 1 to 1200 minutes. The atmospheric gas consists of hydrogen or a mixture of hydrogen and argon, whose dew point is in a range of from −60° C. to +20° C. After the front end of the Ni-base alloy tube reaches the outlet side of the furnace, the supply of atmospheric gas into the tube is switched to the supply from other gas supplying device. The operations are repeated.
REFERENCES:
patent: 5413642 (1995-05-01), Alger
patent: 6482528 (2002-11-01), Anada et al.
patent: 6488783 (2002-12-01), King et al.
patent: 2 267 379 (1975-12-01), None
patent: 50-133910 (1975-10-01), None
patent: 53-6212 (1978-01-01), None
patent: 54-48619 (1979-04-01), None
patent: 64-55366 (1989-03-01), None
patent: 1-159362 (1989-06-01), None
patent: 2-47249 (1990-02-01), None
patent: 2-80552 (1990-03-01), None
patent: 3-153858 (1991-07-01), None
patent: 4-350180 (1992-12-01), None
patent: 11-21629 (1999-01-01), None
patent: 11-256308 (1999-09-01), None
patent: 2002-121630 (2002-04-01), None
patent: 2002-228361 (2002-08-01), None
patent: WO 02/14566 (2002-02-01), None
Anada Hiroyuki
Imoto Toshihiro
Kitamura Kazuyuki
Miyahara Osamu
Buchanan & Ingersoll PC
Sumitomo Metal Industries Ltd.
LandOfFree
Method of heat treatment for Ni-base alloy tube does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of heat treatment for Ni-base alloy tube, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of heat treatment for Ni-base alloy tube will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3650026