Method of heat treating a superalloy component and an alloy...

Metal treatment – Process of modifying or maintaining internal physical... – Heating or cooling of solid metal

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C148S675000

Reexamination Certificate

active

08083872

ABSTRACT:
A method of heat treating a superalloy component includes solution heat treating the component at a temperature below the gamma prime solvus temperature to produce a fine grain structure. Insulation is placed over a first area to form an insulated assembly that is placed in a furnace at a temperature below the solvus temperature and maintained at that temperature for a predetermined time to achieve a uniform temperature. The temperature is increased at a predetermined rate to a temperature above the solvus temperature to maintain a fine grain structure in a first region, produce a coarse grain structure in a second region and produce a transitional structure in a third region between the first and second regions. The insulated assembly is removed from the furnace when the second region has been above the solvus temperature for a predetermined time and/or the first region has reached a predetermined temperature.

REFERENCES:
patent: 5269857 (1993-12-01), Ganesh et al.
patent: 5312497 (1994-05-01), Mathey
patent: 5527020 (1996-06-01), Ganesh et al.
patent: 5571345 (1996-11-01), Ganesh et al.
patent: 6610110 (2003-08-01), Manka
patent: 6660110 (2003-12-01), Gayda et al.
patent: 0284876 (1988-10-01), None
patent: 1813690 (2007-08-01), None

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of heat treating a superalloy component and an alloy... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of heat treating a superalloy component and an alloy..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of heat treating a superalloy component and an alloy... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-4294821

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.