Electrolysis: processes – compositions used therein – and methods – Electrolytic coating – Forming nonelectrolytic coating after depositing...
Patent
1990-09-17
1992-06-23
Niebling, John
Electrolysis: processes, compositions used therein, and methods
Electrolytic coating
Forming nonelectrolytic coating after depositing...
2041811, 2041815, 205109, 205228, C25D 1302, C23C 2800
Patent
active
051240068
ABSTRACT:
A method for coating a heat engine part, particularly a turbo-machine part made of a superalloy and adapted for use in aeronautical applications, comprises electrophoretically depositing a metallic structure of cellular form with uniformly disposed cells of predetermined size. The deposition is performed using an electrophoresis bath containing methanol, aluminum chloride as an electrolyte, and a powder containing Cr, Al, Y, Ta and Ni. The cellular metallic structure is consolidated by a sintering treatment, which may be reactive, or metallization, preferably in the vapor phase, and the coating is completed by applying a ceramic material by plasma spraying.
REFERENCES:
patent: 3486927 (1969-12-01), Gauje
patent: 4152223 (1979-05-01), Wallace et al.
patent: 4248940 (1981-02-01), Goward et al.
patent: 4328285 (1982-05-01), Siemers et al.
patent: 4627896 (1986-12-01), Nazmy et al.
patent: 4810334 (1989-03-01), Honey et al.
Fayeulle Dominque M. M.
Henon Jean-Paul
Morbioli Rene J.
Association pour la Recherche et le Developpement des Methodes e
Leader William T.
Niebling John
Societe Nationale d'Etude et de Construction de Moteurs d'Aviati
LandOfFree
Method of forming heat engine parts made of a superalloy and hav does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of forming heat engine parts made of a superalloy and hav, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of forming heat engine parts made of a superalloy and hav will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-930864