ABSTRACT:
The present invention provides an alloy having improved crack growth inhibition and having high strength at high temperatures. The composition of the alloy is essentially as follows:
REFERENCES:
patent: 3061426 (1962-10-01), Bieber
Davis Jr. James C.
Dean R.
General Electric Company
Magee Jr. James
Rochford Paul E.
LandOfFree
Method of forming fatigue crack resistant nickel base superalloy does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of forming fatigue crack resistant nickel base superalloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of forming fatigue crack resistant nickel base superalloy will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-332654