ABSTRACT:
A method of forming a weld joint between an austenitic stainless steel and a ferritic steel. The ferritic steel contains 0.03 to 0.12% carbon, 0.70% or less silicon, 0.10 to 1.50% manganese, 0.030% or less phosphorus, 0.015% or less sulphur, 1.50 to 3.50% chromium, 0.40% or less molybdenum, 1.00 to 3.00% tungsten, 0.10 to 0.35% vanadium, 0.01 to 0.10% niobium, 0.030% or less Sol. aluminum, 0.020% or less boron, and 0.030% or less nitrogen.

REFERENCES:
patent: 2770030 (1956-11-01), Carpenter et al.
patent: 4525620 (1985-06-01), Deverell et al.
patent: 4703885 (1987-11-01), Lindgren et al.
Koyama, Patent Abstracts of Japan, vol. 10, No. 295 (M-523) [2351], Oct. 7, 1986 & JP-A-61 108477.
King et al., "Development Of An Improved Stainless Steel To Ferritic Steel Transition Joint", Welding Journal, vol. 56, No. 11, Nov. 1977, pp. 354s-358s.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of forming a weld joint of austenitic stainless steel/fer does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of forming a weld joint of austenitic stainless steel/fer, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of forming a weld joint of austenitic stainless steel/fer will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-411188

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.