Adhesive bonding and miscellaneous chemical manufacture – Methods – Surface bonding and/or assembly therefor
Reexamination Certificate
2008-03-17
2010-10-26
Nguyen, Khanh (Department: 1791)
Adhesive bonding and miscellaneous chemical manufacture
Methods
Surface bonding and/or assembly therefor
C056S060000, C056S106000, C056S344000, C056S036000
Reexamination Certificate
active
07819998
ABSTRACT:
There is described a method of forming a touch screen laminate for use in a resistive touch screen display, the method comprising the steps of bonding a layer of ultra-thin glass to a polymer layer by means of an optical adhesive applied uniformly between the glass layer and the polymer layer and applying a non-electrically conductive insulating layer to a lower surface of the polymer layer in a peripherally extending band.
REFERENCES:
patent: 3574030 (1971-04-01), Callander et al.
patent: 4220815 (1980-09-01), Gibson
patent: 5159323 (1992-10-01), Mase
patent: 5445890 (1995-08-01), Bayha et al.
patent: 5838309 (1998-11-01), Robsky et al.
patent: 6287674 (2001-09-01), Verlinden et al.
patent: 6555235 (2003-04-01), Aufderheide et al.
patent: 6556189 (2003-04-01), Takahata
patent: 6809280 (2004-10-01), Divigalpitiya
patent: 2004/0060634 (2004-04-01), Abe et al.
patent: 1139209 (1983-01-01), None
patent: 2359366 (2000-07-01), None
patent: 2370121 (2000-11-01), None
patent: 2038598 (2002-01-01), None
Hoover Matthew
Nguyen Khanh
Sturm & Fix LLP
LandOfFree
Method of forming a touch screen laminate does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of forming a touch screen laminate, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of forming a touch screen laminate will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-4205726