Bright, tarnish resistant and color stable ternary alloys of about 40 - 90% of tin, about 10 - 50% cobalt and about 1 - 28% of a third metal of Periodic Group II.sub.B, III.sub.A or VI.sub.B. Typical third metals are zinc, cadmium, indium, antimony or chromium. The alloys are electrodeposited from aqueous acidic baths at a temperature of about 50.degree. - 85.degree.C. and current density of about 5 - 45 A/ft..sup.2.
REFERENCES:
patent: 2853382 (1958-09-01), Klochkov
patent: 3772168 (1973-11-01), Dillenberg
Federick A. Lowenheim, "Modern Electroplating", pg. 6, 2nd edition, (1963).
Hyner Jacob
Michelson Robert A.
Kaplan G. L.
Whyco Chromium Company Inc.
LandOfFree
Method of electrodepositing an alloy of tin, cobalt and a third does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of electrodepositing an alloy of tin, cobalt and a third , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of electrodepositing an alloy of tin, cobalt and a third will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1275634