ABSTRACT:
The present invention deals with alloys consisting essentially of the elements nickel, iron and boron. Boron is present at from 0.1 to 2.0% by weight; iron is present from 17 to 27% by weight and the balance is nickel. The alloy has high resistance to corrosion and H.sub.o and H.sub.c are less than 0.1 Oe in films 3000.ANG. thick. It is prepared by electrodeposition from a bath having a pH of 2.5 or less, and containing a borane reducing agent.

REFERENCES:
patent: 3483029 (1969-12-01), Koretzky et al.
patent: 3485725 (1969-12-01), Koretzky
W. O. Freitag et al., J. Electrochem. Soc., III, No. 1, pp. 35-39, (Jan. 1964).

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of electrodepositing a low coercine force, corrosion-resi does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of electrodepositing a low coercine force, corrosion-resi, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of electrodepositing a low coercine force, corrosion-resi will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-665993

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.