ABSTRACT:
A method of joining superalloy substrates together comprises diffusion bonding the superalloy substrates by depositing an activator directly on the surface of the joint to be bonded and thereafter subjecting the joint to heat and pressure. The heat and pressure causes the surface of the superalloy, in the presence of the activator, to diffusion bond without the use of a brazing alloy. By eliminating the brazing alloy, a high strength, high temperature bond is achieved, yet there is no molten brazing alloy to be drawn through capillary action into any fine features surrounding the joint being bonded, and there is no residue left at the interface that would diminish the mechanical or chemical properties of the joint.
REFERENCES:
patent: 3628226 (1971-12-01), Nelson
patent: 3971875 (1976-07-01), Regalbuto
patent: 4055988 (1977-11-01), Dutton, Jr.
patent: 4059217 (1977-11-01), Woodward
patent: 4087037 (1978-05-01), Schier et al.
patent: 4474044 (1984-10-01), Leistner et al.
patent: 5431804 (1995-07-01), Caballero
patent: 5735448 (1998-04-01), Draghi et al.
patent: 5933951 (1999-08-01), Bergue et al.
patent: 6337471 (2002-01-01), Kistner et al.
patent: 6464129 (2002-10-01), Stueber et al.
patent: 20020104875 (2002-08-01), Stueber et al.
patent: 20030152705 (2003-08-01), Pfaendtner et al.
patent: 20040115355 (2004-06-01), Bauer et al.
patent: 20040169063 (2004-09-01), Stueber et al.
Blanche Brenton L.
Stueber Richard J.
Stoner Kiley S.
Titus John D.
Triumph Brands, Inc.
LandOfFree
Method of diffusion bonding superalloy laminates does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of diffusion bonding superalloy laminates, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of diffusion bonding superalloy laminates will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3391809