ABSTRACT:
A method of applying a duplex sheet cladding to a structural substrate is disclosed. The method utilizes hot isostatic pressure with molten glass as a pressure transmitting medium. An inner sheet cladding of aluminum is formed over the substrate and then an outer MCrAlY sheet cladding is assembled thereon which completely envelops and seals the inner cladding. Thereafter the duplex cladding is diffusion bonded to the substrate at elevated pressures and temperatures in accordance with a programmed time-temperature hot isostatic pressure cycle.
REFERENCES:
patent: 3649225 (1974-03-01), Simmons, Jr.
patent: 3849865 (1974-11-01), Gedwill et al.
patent: 3873347 (1975-03-01), Walker et al.
patent: 3874901 (1975-04-01), Rairden
patent: 3904101 (1975-09-01), Beltran et al.
patent: 3928901 (1975-12-01), Schilling et al.
patent: 3952939 (1976-04-01), Schilling et al.
Beltran Adrian M.
Schilling William F.
Ahern John F.
Cutter Lawrence D.
General Electric Company
Hall Carl E.
Ramsey K. J.
LandOfFree
Method of diffusion bonding duplex sheet cladding to superalloy does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of diffusion bonding duplex sheet cladding to superalloy , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of diffusion bonding duplex sheet cladding to superalloy will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1424474