ABSTRACT:
An article with an improved buffer layer architecture includes a substrate having a textured metal surface, and an electrically conductive lanthanum metal oxide epitaxial buffer layer on the surface of the substrate. The article can also include an epitaxial superconducting layer deposited on the epitaxial buffer layer. An epitaxial capping layer can be placed between the epitaxial buffer layer and the superconducting layer. A method for preparing an epitaxial article includes providing a substrate with a metal surface and depositing on the metal surface a lanthanum metal oxide epitaxial buffer layer. The method can further include depositing a superconducting layer on the epitaxial buffer layer, and depositing an epitaxial capping layer between the epitaxial buffer layer and the superconducting layer.

REFERENCES:
patent: 5270298 (1993-12-01), Ramesh
patent: 5418081 (1995-05-01), Kawasaki et al.
patent: 5470668 (1995-11-01), Wu et al.
patent: 5739086 (1998-04-01), Goyal et al.
patent: 5856276 (1999-01-01), Koshy et al.
patent: 5872080 (1999-02-01), Arendt et al.
patent: 6027826 (2000-02-01), deRochemont et al.
patent: 6077344 (2000-06-01), Shoup et al.
patent: 6117571 (2000-09-01), Baum et al.
patent: 6296701 (2001-10-01), Christen et al.
patent: 6351006 (2002-02-01), Yamakawa et al.
patent: 6428635 (2002-08-01), Fritzemeier et al.
patent: 6440211 (2002-08-01), Beach et al.
patent: 6455166 (2002-09-01), Truchan et al.
patent: 6458223 (2002-10-01), Hans Thieme et al.
patent: 6475311 (2002-11-01), Fritzemeier et al.
patent: 6663976 (2003-12-01), Beach et al.
patent: 6673387 (2004-01-01), Zhang et al.
M. Paranthaman, et al., “Growth of blaxially textured buffer layers on rolled-Ni substrates by electron beam evaporation”, Physica C 275 (1997) pp. 266-272.
Frank McNally, et al., “Fatigue properties of lanthanum strontium manganate-lead zirconate titanate epitaxial thin film heterostructures produced by a chemical solution deposition method” J. Mater Res., vol. 15, No. 7, Jul. 2000, pp. 1546-1550.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of depositing an electrically conductive oxide buffer... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of depositing an electrically conductive oxide buffer..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of depositing an electrically conductive oxide buffer... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3441616

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.