ABSTRACT:
The molecular weight of acrylic acid-acrylamide copolymers can be controlled between the range of 3,000-300,000 by polymerizing an aqueous solution of these comonomers in a tube reactor at a pressure between 50-350 psig in the presence of a free radical catalyst and with the following reaction parameters being specified; monomer solids, initiation temperature, monomer pH, initiator concentration, acrylic acid-acrylamide monomer ratio, and residence time in the reactor.
REFERENCES:
patent: 3035033 (1962-05-01), Schweitzer et al.
patent: 3658772 (1972-04-01), Volk et al.
patent: 3872063 (1975-03-01), Kim
patent: 3929739 (1975-12-01), Barabas et al.
Goretta Louis A.
Otremba Robert R.
Miller Robert A.
Nalco Chemical Company
Premo John G.
Wong, Jr. Harry
LandOfFree
Method of controlling the molecular weight of vinyl carboxylic a does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of controlling the molecular weight of vinyl carboxylic a, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of controlling the molecular weight of vinyl carboxylic a will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-922111