ABSTRACT:
In continuously casting molten steel at least a pair of rolls is disposed near the leading end of the crater at which solidification of the molten steel in the cast piece completes so as to roll the cast piece at a reduction rate of from 0.1 to 2.0%. The variation in the thickness of the cast piece is detected and compared with a definite reference value for controlling the drawing speed and or the quantity of the secondary cooling water.
REFERENCES:
patent: 3812900 (1974-05-01), Bollig et al.
Kawawa Takaho
Miyahara Shinobu
Sato Hideki
Drucker William Anthony
Hampilos Gus T.
Husar Francis S.
Nippon Kokan Kabushiki Kaisha
LandOfFree
Method of continuously casting steel does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of continuously casting steel, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of continuously casting steel will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-647702