ABSTRACT:
A method for concentrating a fine coal slurry having an average particle diameter of 250 microns or less is provided in which the slurry is fed to a liquid-permeable membrane separator which provides a high rate of shear flow horizontal to the membrane. The feed may be heated to increase the flow rate, and crossflow across the membrane may be pulsed to prevent clogging of the membrane. Dispersant may also be added to improve the flow.
REFERENCES:
patent: 4593859 (1986-06-01), Nakaoji et al.
patent: 4634451 (1987-01-01), Lipowski et al.
patent: 4645514 (1987-02-01), Lane et al.
patent: 4687490 (1987-08-01), Heaton, III et al.
patent: 4765781 (1988-08-01), Wilks et al.
patent: 4810259 (1989-03-01), Rakitsky et al.
patent: 4952317 (1990-08-01), Culkin
patent: 5182014 (1993-01-01), Goodman
patent: 5277368 (1994-01-01), Kindig
LandOfFree
Method of concentrating fine coal slurries does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of concentrating fine coal slurries, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of concentrating fine coal slurries will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1946189