Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – At least one aryl ring which is part of a fused or bridged...
Reexamination Certificate
2005-05-31
2005-05-31
Cheung, William K. (Department: 1713)
Synthetic resins or natural rubbers -- part of the class 520 ser
Synthetic resins
At least one aryl ring which is part of a fused or bridged...
C526S352000
Reexamination Certificate
active
06900266
ABSTRACT:
Method of compounding a multimodal polyethylene composition in a compounding device, wherein a) the total residence time of the polyethylene composition in the compounding device is at least 1.5 minutes, b) the total drive specific energy (SEC) applied on the polyethylene composition is from 0.270 to 0.460 kWh/kg, c) optionally, a specific cooling energy (SCC) of at most 0.200 kWh/kg is applied on the polyethylene composition, d) the total specific energy, which is the difference between the total drive specific energy SEC and any specific cooling energy SCC, applied on the polyethylene composition is from 0.220 to 0.330 kWh/kg.
REFERENCES:
patent: 3381060 (1968-04-01), Peacock et al.
patent: 5336573 (1994-08-01), Zuckerbrod et al.
patent: 0 645 232 (1995-03-01), None
patent: 0 713 889 (1996-05-01), None
patent: WO 00/01473 (2000-01-01), None
Cheung William K.
Finnegan, Henderson Farabow, Garrett and Dunner L.L.P.
Solvay Polyolefins Europe-Belgium
LandOfFree
Method of compounding a multimodal polyethylene composition does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of compounding a multimodal polyethylene composition, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of compounding a multimodal polyethylene composition will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3393429