ABSTRACT:
A method and related apparatuses are disclosed for coating an elongated filament, such as wire, wherein wire is coated with a heated coating material, such as polyetheretherketone (PEEK), and the coated wire is maintained at a temperature and for a period of time sufficient for a desired quantity and size of crystals to form in the coating material and to minimize internal residual stress. Thereafter, the coated wire is rapidly cooled to a temperature below its crystallization temperature, such as in a quenching bath. A crystalline PEEK coating results which has minimized internal residual stress, is less brittle, and has improved cracking, peeling and abrasion resistance over amorphous PEEK coating obtainable using prior methods.

REFERENCES:
patent: 3849192 (1974-11-01), Schmidt
patent: 4391848 (1983-07-01), Hilker
patent: 4606870 (1986-08-01), McGregor
patent: 5075136 (1991-12-01), Nield et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of coating elongated filaments does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of coating elongated filaments, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of coating elongated filaments will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1141393

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.