Coating processes – Nonuniform coating – Deforming the base or coating or removing a portion of the...
Patent
1994-05-17
1995-06-06
Bell, Janyce
Coating processes
Nonuniform coating
Deforming the base or coating or removing a portion of the...
4272481, 427249, 427255, 427277, 427287, 427290, 427292, 427370, 427585, B05D 312
Patent
active
054221404
ABSTRACT:
There is now provided a method of manufacturing a coated ceramic body with improved performance when used as a tool insert for metal cutting purposes. By subjecting the body after the coating to a hot isostatic pressing operation at a pressure of 10-300 MPa and a temperature of >1200.degree. C., an improved adherence of the coating has been achieved. The method is particularly applicable to whisker-reinforced ceramic composites.
REFERENCES:
patent: 4332458 (1982-03-01), Siebmanns
patent: 4539231 (1985-09-01), Betz et al.
patent: 4619866 (1986-10-01), Smith et al.
patent: 4801510 (1989-01-01), Mehrotra et al.
patent: 4820663 (1989-04-01), Mehrotra et al.
patent: 4997683 (1991-03-01), Wright
Bell Janyce
Sandvik AB
LandOfFree
Method of coating a ceramic body does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of coating a ceramic body, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of coating a ceramic body will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-985983