Glass manufacturing – Processes – With destruction or delamination of transitory attached or...
Reexamination Certificate
2005-02-22
2005-02-22
Vincent, Sean (Department: 1731)
Glass manufacturing
Processes
With destruction or delamination of transitory attached or...
C065S060200, C065S060300, C065S061000, C065S114000
Reexamination Certificate
active
06857290
ABSTRACT:
An index-matching coating is applied directly to a low-emissivity (“lowE”) thin-film coating. Nodules growing from a site in the lowE coating are removed to avoid propagation of defects through the layers of the index-matching coating. A tempering step in an oxygen-containing atmosphere produces compressive stress in the lowE coating and hardens the coating. The compressive stress facilitates removal of the nodules and the hardening allows mechanical cleaning of the lowE coating prior to the index-matching coating, further removing nodules. Magnesium-fluoride is used as the final layer of the index-matching coating in one embodiment to improve abrasion resistance. The resulting glass panel may be used as a display panel in a plasma display or an organic light-emitting diode display, for example.
REFERENCES:
patent: 3034916 (1962-05-01), Eshner
patent: 4466992 (1984-08-01), Dreiling
patent: 4790922 (1988-12-01), Huffer
patent: 4806220 (1989-02-01), Finley
patent: 4989789 (1991-02-01), Moruno
patent: 5010037 (1991-04-01), Lin et al.
patent: 5059295 (1991-10-01), Finley
patent: 5213880 (1993-05-01), Yabuchi
patent: 5272133 (1993-12-01), Josefowicz et al.
patent: 5378506 (1995-01-01), Imai et al.
patent: 5558946 (1996-09-01), Nishimoto
patent: 5645885 (1997-07-01), Nishimoto
patent: 5804102 (1998-09-01), Oi et al.
patent: 5821001 (1998-10-01), Arbab et al.
patent: 5920080 (1999-07-01), Jones
patent: 5942338 (1999-08-01), Arbab et al.
patent: 6024084 (2000-02-01), Gerhardinger
patent: 6069443 (2000-05-01), Jones et al.
patent: 6146225 (2000-11-01), Sheats et al.
patent: 6188174 (2001-02-01), Marutsuka
patent: 6197408 (2001-03-01), Kanbara et al.
patent: 6207266 (2001-03-01), Kanbara et al.
patent: 6214422 (2001-04-01), Yializis
patent: 6229085 (2001-05-01), Gotoh et al.
patent: 6251800 (2001-06-01), Sun et al.
patent: 6258637 (2001-07-01), Wilk et al.
patent: 6266037 (2001-07-01), Flasck
patent: 6270832 (2001-08-01), Honda et al.
patent: 6410173 (2002-06-01), Arfsten et al.
patent: 6410887 (2002-06-01), Reunamaki
patent: 6469685 (2002-10-01), Woodruff et al.
patent: 6472073 (2002-10-01), Singh et al.
patent: 6475626 (2002-11-01), Stachowiak
patent: 6495251 (2002-12-01), Arbab et al.
Adair Robert W.
Duffy Brad A.
Allen Dyer Doppelt Milbrath & Gilchrist, P.A.
JDS Uniphase Corporation
Vincent Sean
LandOfFree
Method of applying barrier coatings to glass panels does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of applying barrier coatings to glass panels, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of applying barrier coatings to glass panels will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3485512