ABSTRACT:
Coal tar pitch is liquified at temperature of from about 135.degree. C. to 280.degree. C. The liquid coal tar pitch is filtered through a sieve with apertures from about 100 to 220 .mu.m and with a closed surface area of at least 75 percent of the total sieve surface under pressures of from about 2 to 10 bar until a filter cake of a height of from about 40 to 80 mm forms above the sieve for separating ash, soot and quinoline insoluble particles from the liquid. Then the filtrate obtained is subjected to a coking process.
The needle cokes resulting in accordance with the invention provide excellent materials for the production of graphite electrodes.
REFERENCES:
patent: Re25467 (1963-10-01), Logan
patent: 4104150 (1978-08-01), Romey
patent: 4111794 (1978-09-01), Pietzka
Kokot Hellmut
Kolling Georg
Romey Ingo
Bergwerksverband GmbH
Striker Michael J.
Tufariello T. M.
LandOfFree
Method for the production of needle coke does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for the production of needle coke, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for the production of needle coke will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-552130