ABSTRACT:
Method for the production of a wear resistant part of a soil working tool comprising forming a mixture of 67-90% by volume of iron particles consisting of at least 97% Fe and 10-33% by volume of hard particles having a desired particle size distribution, and subsequently pressing the mixture at a pressure of at least 3500 kp/cm.sup.2 to form a compact, sintering the compact at a temperature of 900.degree.-1200.degree. C., and optionally sinter forging the sintered compact. The sintered part consists of an iron matrix in which hard particles with a predetermined particle size distribution are embedded.
REFERENCES:
patent: 2672426 (1954-03-01), Grubel et al.
patent: 3493351 (1970-02-01), Bergna et al.
patent: 3809540 (1974-05-01), Mal
patent: 3967935 (1976-07-01), Frehn
R. C. D. Richardson, "The Wear of Metallic Materials by Soil-Practical Phenomena", in J. Agric Engng. Res. (1967) 12 (1), 22-39.
Lechert Jr. Stephen J.
Teknologisk Institut
LandOfFree
Method for the production of a wear resistant part of a soil wor does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for the production of a wear resistant part of a soil wor, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for the production of a wear resistant part of a soil wor will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1673419