ABSTRACT:
Equipment used in a substantially water free, but corrosive environment is protected from corrosion by coating only certain welded parts thereof with a metal more base than the metal part coated.
REFERENCES:
patent: 3058206 (1962-10-01), Mets
patent: 3922396 (1975-11-01), Speivs
Evans, An Introduction to Metal Corrosion, Edward Arnold & Co., London, 1948, p. 123.
Kirk-Othmer, Encyclopedia of Chemical Technology, vol. 6, John Wiley & Son, pp. 298, 303.
Kawakami Katsuhiko
Yamaguchi Kineo
Kendall Ralph S.
Nippon Mining Co., Ltd.
LandOfFree
Method for the prevention of stress corrosion cracking does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for the prevention of stress corrosion cracking, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for the prevention of stress corrosion cracking will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-652278