ABSTRACT:
An alloy of nickel and titanium in the atomic ratio of 49:51 to 56:44 can be prepared at a temperature much lower than the eutectic point of the corresponding alloy. Thus, a green compact of a powdery mixture of the component metals is subjected to a heat treatment under high vacuum first at a rate of temperature elevation of 5.degree. to 30.degree. C./minute up to a temperature of, for example, 600.degree. C. and then at a rate of temperature elevation of at least 40.degree. C./minute up to a temperature of 815.degree.-900.degree. C. The surface of the metal particles is activated at the first stage along with degassing and the surface-activated metal particles are brought into an exothermic reaction at the second stage to cause explosive fusion and alloying.
REFERENCES:
patent: 3950166 (1976-04-01), Obara et al.
patent: 4478790 (1984-10-01), Huther et al.
patent: 4657822 (1987-04-01), Goldstein
Suzuki Yoshikazu
Unuma Hidero
Agency of Industrial Science and Technology
Lechert Jr. Stephen J.
LandOfFree
Method for the preparation of an alloy of nickel and titanium does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for the preparation of an alloy of nickel and titanium, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for the preparation of an alloy of nickel and titanium will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-920448