ABSTRACT:
The invention concerns a method for the manufacture of a superconductor with a layer of the A-15 phase of the system Nb--Al or Nb--Al--Ge. According to the invention, a niobium carrier is provided with a 0.5 to 5 .mu.m thick layer consisting of NbAl.sub.3 and Al or of Nb(Al,Ge).sub.3, respectively, by being placed in an aluminum melt which is saturated with niobium or niobium and germanium, respectively, and is heated to 800.degree. to 1400.degree. C, and the niobium carrier provided with this layer is then annealed in an inert atmosphere for 0.5 to 5 seconds at a temperature of 1700.degree. to 1960.degree. C.
REFERENCES:
patent: 2216519 (1940-10-01), Quarnstrom
patent: 3346467 (1967-10-01), Allen
patent: 3694274 (1972-09-01), Giorgi et al.
patent: 3765930 (1973-10-01), Miyano
Journal Appl. Physics, vol. 43, 1972, pp. 2407-2412.
Metallurgical Transactions, vol. 3, May 1972, pp. 1177-1181.
Zeitschrift Fur Naturforschung, 25a, 1970, pp. 1659-1669.
Constitution of Binary Alloys, Second Supplement Shunk, 1969, pp. 18-20.
Fink Arno
Muller Alfred
Lovell C.
Siemens Aktiengesellschaft
LandOfFree
Method for the manufacture of a superconductor with a layer of t does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for the manufacture of a superconductor with a layer of t, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for the manufacture of a superconductor with a layer of t will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-104126