ABSTRACT:
A method for applying a heat insulation layer (11, 12, 13) or a metallic protective layer to a thermally stressed component (200) having a basic material (10) in order to eliminate local damage (14) or an untreated place in the coating, includes, in a first step, pretreating the local damage (14) or untreated place, and, in a second step, applying layers (17, 18) necessary for eliminating the local damage (14) or untreated place. A markedly improved lifetime of the processed component can be achieved in that, within the first step, the edge regions (15) of the layers (11, 12, 13) ending at the local damage (14) or untreated place are processed so that they form uniformly sloped and terrace-shaped edge regions (16). Furthermore, a precharacterization of the entire coated region of the operationally stressed component or critical places by FSECT makes it possible to reduce the risk in terms of otherwise overlooked layer regions, the remaining lifetime of which would not persist for the following operating time.
REFERENCES:
patent: 5667700 (1997-09-01), Rudigier et al.
patent: 5735448 (1998-04-01), Draghi et al.
patent: 5958166 (1999-09-01), Walters et al.
patent: 6042880 (2000-03-01), Rigney et al.
patent: 6203847 (2001-03-01), Conner et al.
patent: 6235352 (2001-05-01), Leverant et al.
patent: 6274193 (2001-08-01), Rigney et al.
patent: 6305077 (2001-10-01), Conner et al.
patent: 6465040 (2002-10-01), Gupta et al.
patent: 6605364 (2003-08-01), Conner et al.
patent: 6637643 (2003-10-01), Hasz et al.
patent: 6707297 (2004-03-01), Nath et al.
patent: 7309512 (2007-12-01), Srinivasan
patent: 2003/0082297 (2003-05-01), Wolkers et al.
patent: 2007/0231474 (2007-10-01), Srinivasan
patent: 0808913 (1997-11-01), None
patent: 1217090 (2002-06-01), None
patent: 1408134 (2004-04-01), None
patent: 2005/106075 (2005-11-01), None
Search Report for EP Patent App. No. 04101784.9 (Aug. 25, 2004).
International Search Report for PCT Patent App. No. PCT/EP2005/051748 (Sep. 15, 2005).
Duda Thomas
Kiliani Stefan
Stankowski Alexander
Szücs Frigyes
ALSTOM Technology Ltd.
Cermak Adam J.
Cermak Kenealy Vaidya & Nakajima LLP
Everhart Caridad M
LandOfFree
Method for the application of a protective coating to a... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for the application of a protective coating to a..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for the application of a protective coating to a... will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-4146190