ABSTRACT:
In the method for stabilizing an artificial patina layer produced on a copper panel, a transparent cover layer consisting of water glass and hydroxycellulose is applied onto the patina layer immediately after it is produced. The cover layer can consist of sodium or potassium water glass and hydroxycellulose, and is applied onto an artificially patinated copper panel by either immersion or spraying. After immersion or spraying, the cover layer is dried. This occurs in an atmosphere with a temperature of approximately 20.degree. C. to 150.degree. C., within a time period of approximately one to one and a half hours.

REFERENCES:
patent: 1012887 (1911-12-01), Medveczky
patent: 2339200 (1944-01-01), Sowa
patent: 2350161 (1944-05-01), Gloor
patent: 3960576 (1976-06-01), Carter et al.
patent: 4341878 (1982-07-01), Marcantonio et al.
Translation of JP 64-004492, Jan. 1989.
Translation of JP 5-098497, Apr. 1993.
Translation of FR 1527052.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for stabilizing a patina layer does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for stabilizing a patina layer, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for stabilizing a patina layer will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1318467

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.