ABSTRACT:
Solidification of colloidal argillaceous matter in essentially non-settling, aqueous slime media into a solid stable matrix is accomplished by mixing such slime with a hydratable calcium sulfate and hydrating to form an interlocking strength bearing matrix. The method is particularly useful for coalescing phosphatic clay slimes with hydratable calcium sulfate prepared from the co-produced waste phosphogypsum.

REFERENCES:
patent: 3761239 (1973-09-01), Cook et al.
patent: 3876439 (1975-04-01), Schneider
patent: 3947284 (1976-03-01), Kitsugi et al.
patent: 3980489 (1976-09-01), Schneider
patent: 3980490 (1976-09-01), Schneider

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for solidifying waste slime suspensions does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for solidifying waste slime suspensions, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for solidifying waste slime suspensions will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1629370

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.