ABSTRACT:
Age-hardened aluminum alloy sheet can be subjected to a shearing operation, such as trimming or piercing, with reduced sliver formation by first heating the region to be sheared to a temperature above about 250.degree. C., immediately quenching the heated region to soften the region, and then performing the shearing operation in the softened region before age-hardening occurs.
REFERENCES:
patent: 3856584 (1974-12-01), Cina
patent: 4235646 (1980-11-01), Neufeld et al.
patent: 4614552 (1986-09-01), Fortin et al.
patent: 4766664 (1988-08-01), Benedyk
Elve M. Alexandra
General Motors Corporation
Grove George A.
Ryan Patrick
LandOfFree
Method for sliver elimination in shearing aluminum sheet does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for sliver elimination in shearing aluminum sheet, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for sliver elimination in shearing aluminum sheet will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-361279