Metal deforming – By shot-blasting
Patent
1981-09-10
1984-06-19
Crosby, Gene P.
Metal deforming
By shot-blasting
C21D 706
Patent
active
044547404
ABSTRACT:
A method for simultaneously shot peening and smoothing includes use of relatively large, smooth, hard, spherical steel shot having a substantially uniform diameter in the range 1-2.5 mm. Titanium workpieces are provided in one step with a compressive stress layer of the order of 0.13 mm and a surface finish of better than 15.times.10.sup.-6 inch AA, compared to conventional peened finishes of the order of 40.times.10.sup.-6 inch AA. Surface finish and peening intensity are inter-related and dependent on shot diameter, mass, velocity, and energy within relatively small limits. The shot diameter is uniform within .+-.0.05 mm; the shot impact velocity is uniform within .+-.4 percent or less, in the range 1.4-12 m/s.
REFERENCES:
patent: 937180 (1909-10-01), Ridd
patent: 3705511 (1972-12-01), Brandel
patent: 4034585 (1977-07-01), Straub
Carlin, "What Makes a Good Steel Shot", Metal Progress; Jun. '59; pp. 83-85.
Person, "Effect of Shot Peening Variables . . . ," Metal Progress; Jun. '81, pp. 33-35.
ASM "Shot Peening," Metals Handbook, vol. 2, pp. 398-405, (1964), Amer. Soc. for Metals.
Pope, Mohamed "Residual Plastic Strains . . . ," Jnl. Iron & Steel Inst., vol. 180, pp. 285-297 (Jul. 1955).
Kurz, "The Merits of Shot Peening," Production, pp. 107-111.
Kurz, "Shot Peening," Modern Machine Shop, (Jun. 1967), pp. 4-12; 20-23; 32-35.
Robertson, "The Effects of Shot Size on Residual . . . ," No. 710284 (Sep. 1968), SAE Transactions.
Brandel, Klass "Ball Forming Solves Contouring Problems," Metal Progress, (Mar. 1971), pp. 56-57.
Mock "Mechanical Finishes Brighten . . . ," Materials Engineering (Sep. 1968), pp. 64-66.
Pangborn Corp., "Shot Peening".
Metal Improvement Corp., "Shot Peening Applications," 6th Ed., (1980), pp. 3-10; 17;25-27;35.
Soc. Auto. Engineers, AMS-2430H Specification, (1972), pp. 1-15.
U.S. Gov't. Military Specification Mils-13165B, (Dec. 1966), pp. 1-22.
Loersch Joseph F.
Neal James W.
Crosby Gene P.
Nessler C. G.
United Technologies Corporation
LandOfFree
Method for simultaneous peening and smoothing does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for simultaneous peening and smoothing, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for simultaneous peening and smoothing will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-409235