ABSTRACT:
A method for forming or remanufacturing a component to have an internal space. A refractory metal blocking element is formed, in situ, with at least a portion to be within the internal space. A material is added by at least one of welding, laser cladding, and diffusion brazing, the blocking element at least partially blocking entry of the material to the internal space. The blocking element is removed.

REFERENCES:
patent: 3809553 (1974-05-01), Peaslee
patent: 4008844 (1977-02-01), Duvall et al.
patent: 4285459 (1981-08-01), Baladjanian et al.
patent: 4726104 (1988-02-01), Foster et al.
patent: 4822248 (1989-04-01), Wertz et al.
patent: 5732467 (1998-03-01), White et al.
patent: 5783318 (1998-07-01), Biondo et al.
patent: 5935718 (1999-08-01), Demo et al.
patent: 6049978 (2000-04-01), Arnold
patent: 6503349 (2003-01-01), Pietruska et al.
patent: 6530971 (2003-03-01), Cohen et al.
patent: 6742698 (2004-06-01), Shah et al.
patent: 6986810 (2006-01-01), Behi
patent: 2003/0226878 (2003-12-01), Shah et al.
patent: 2005/0061858 (2005-03-01), Ditzel et al.
patent: 2006/0248718 (2006-11-01), Szela et al.
patent: 597512 (1978-03-01), None
patent: 03/048528 (2003-06-01), None
Patent Abstracts of Japan, vol. 013, No. 122, Mar. 27, 1989 (JP 63295802) (Toshiba Corp.), Dec. 2, 1988.
Patent Abstracts of Japan, vol. 006, No. 056, Apr. 13, 1982 (JP 56167802) (Toshiba Corp.), Dec. 23, 1981.
Patent Abstracts of Japan, vol. 004, No. 084, Jun. 17, 1980 (JP 55042129) (Hitachi Corp.), Mar. 25, 1980.
Patent Abstracts of Japan, vol. 2003, No. 12, Dec. 5, 2003 (JP 2004084604) (Mitsubishi Heavy Ind. Ltd.), Mar. 18, 2004.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for repairing superalloy components using inserts does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for repairing superalloy components using inserts, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for repairing superalloy components using inserts will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2693804

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.