Method for repair of a nickel-base superalloy article using...

Stock material or miscellaneous articles – All metal or with adjacent metals – Composite; i.e. – plural – adjacent – spatially distinct metal...

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C428S636000, C428S544000, C428S926000, C029S889100, C029S402010, C029S402090, C029S402130, C029S402160, C029S402180, C148S527000, C228S119000, C228S262300

Reexamination Certificate

active

06982123

ABSTRACT:
A nickel-base superalloy article, such as a gas turbine stationary flowpath shroud that has previously been in service, is repaired by applying a restoration coating to a surface of the article. The restoration coating is applied by providing a precursor mixture, wherein the precursor mixture has no more than about 15 weight percent chromium and no more than about 0.01 percent yttrium, and wherein the precursor mixture includes a higher-melting-point alloy component and a lower-melting-point alloy component. The precursor mixture is applied to the surface of the article, in a form such as a preform of the alloy components. The article with the precursor mixture applied to the surface thereof is heated to a sufficiently high temperature to melt the lower-melting-point alloy component, thereby forming the restoration coating on the surface of the article.

REFERENCES:
patent: 4073639 (1978-02-01), Duvall et al.
patent: 4381944 (1983-05-01), Smith et al.
patent: 4830934 (1989-05-01), Ferrigno et al.
patent: 5240491 (1993-08-01), Budinger et al.
patent: 5561827 (1996-10-01), Reeves et al.
patent: 5916518 (1999-06-01), Chesnes
patent: 6233822 (2001-05-01), Grossklaus, Jr. et al.
patent: 6464128 (2002-10-01), Messelling et al.
patent: 0 095 668 (1983-12-01), None
patent: 0 293 695 (1988-12-01), None
patent: 1 226 896 (2002-07-01), None
patent: 1 491 283 (2004-12-01), None
patent: WO 97/37800 (1997-10-01), None

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for repair of a nickel-base superalloy article using... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for repair of a nickel-base superalloy article using..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for repair of a nickel-base superalloy article using... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3529543

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.