Cleaning and liquid contact with solids – Processes – Including distortion or deformation of work
Patent
1983-07-13
1985-02-26
Caroff, Marc L.
Cleaning and liquid contact with solids
Processes
Including distortion or deformation of work
134 35, B08B 310, B08B 704
Patent
active
045016216
ABSTRACT:
A coating layer, such as a photosensitive selenium coating is removed from a substrate by producing cracks in the layer, introducing a volume expansive material into the cracks, and then causing the volume expansive material introduced into the cracks to expand and thereby dislodge the coating layer from the substrate.
REFERENCES:
patent: 1898809 (1933-02-01), Berg
patent: 3056700 (1962-10-01), Osterlin
patent: 3419427 (1968-12-01), Plock
patent: 3455737 (1969-07-01), Seibert
patent: 3743692 (1973-07-01), Vinton et al.
patent: 3837815 (1974-09-01), Bixby
patent: 3990907 (1976-11-01), Endo et al.
patent: 4257820 (1981-03-01), Jacobs
Abe Naoto
Akimoto Hidetoshi
Nomori Hiroyuki
Bierman Jordan B.
Caroff Marc L.
Konishiroku Photo Industry Co,., Ltd.
LandOfFree
Method for removing a selenium layer from a substrate does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for removing a selenium layer from a substrate, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for removing a selenium layer from a substrate will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-515497