Method for removing a scale from a superalloy surface

Cleaning and liquid contact with solids – Processes – For metallic – siliceous – or calcareous basework – including...

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

134 21, 134 2213, 134 27, 134 30, B08B 310

Patent

active

043176852

ABSTRACT:
A method for removing scale, particularly oxide scale, from a surface of a high temperature alloy, the surface having been exposed to high temperature conditions, employs an aqueous alkaline hydroxide solution in contact with the scale in an autoclave. The solution is heated in the autoclave in a non-oxidizing atmosphere at a temperature in the range of about 200.degree.-340.degree. C. while providing relative movement between the solution and the scale. Thereafter, the scale reaction product is flushed from the surface to remove the alkaline solution.

REFERENCES:
patent: 2796366 (1957-06-01), Carter
patent: 3121026 (1964-02-01), Beigay et al.
patent: 3126301 (1964-03-01), Faler
patent: 4073662 (1978-02-01), Borom
patent: 4134777 (1979-01-01), Borom
patent: 4188237 (1980-02-01), Chasteen

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for removing a scale from a superalloy surface does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for removing a scale from a superalloy surface, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for removing a scale from a superalloy surface will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-58673

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.