ABSTRACT:
The outer surface of a butt-welded joint is build-up welded such that a ratio h/t is higher than approximate 0.2 and a ratio L/.sqroot.Rt is higher than approximate 1, where h denotes height of a build-up welded portion; t, wall thickness of a pipe; L, width of the build-up welded portion; and R, radius of the pipe. As a result, the residual stresses in the build-up welded portion counterbalances the residual stresses in the welded joint, whereby the residual stresses at the inner surface of the welded joint can be relieved.

REFERENCES:
patent: 4049186 (1977-09-01), Hanneman et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for relieving residual stresses by build-up welding over does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for relieving residual stresses by build-up welding over , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for relieving residual stresses by build-up welding over will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-142582

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.