ABSTRACT:
A method for improving the microstructure of prealloyed titanium alloy compacted articles which comprises the steps of hydrogenating the article at a temperature of about 780.degree. to 1020.degree. C. to a hydrogen level of about 0.50 to 1.50 weight percent, cooling the thus-hydrogenated article to room temperature at a controlled rate, heating the thus-cooled, hydrogenated article to a temperature of about 650.degree. to 750.degree. C. and applying a vacuum to dehydrogenate the article.

REFERENCES:
patent: 4534808 (1985-08-01), Eylon et al.
patent: 4536234 (1985-08-01), Eylon et al.
patent: 4680063 (1987-07-01), Vogt et al.
Kerr et al. in Titanium '80, ed. Kimura et al. Met.Soc.Aime, Warrendale, PA, 1980, pp. 2477-2486.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for refining microstructures of prealloyed titanium powde does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for refining microstructures of prealloyed titanium powde, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for refining microstructures of prealloyed titanium powde will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1728497

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.