ABSTRACT:
A method for reducing the residual acrylic acid present in water-insoluble polyacrylic acid water absorbent gel polymers which comprises treating these polymers with at least 0.5 mole of either amino acid cysteine or lysine per mole of acrylic acid present in said waters for at least 15 minutes at a temperature of at least 80.degree. C.

REFERENCES:
patent: 4320040 (1982-03-01), Fujita et al.
patent: 4339373 (1982-07-01), Robinson
patent: 4525509 (1985-06-01), Hunter et al.
patent: 4604411 (1986-08-01), Yada et al.
patent: 4654039 (1987-03-01), Brandt et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for reducing residual acrylic acid in acrylic acid polyme does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for reducing residual acrylic acid in acrylic acid polyme, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for reducing residual acrylic acid in acrylic acid polyme will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-836398

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.