ABSTRACT:
A process for treating retention pond sludge containing greater than 20% solids including minerals and bitumen and associated with the aqueous extraction of bitumen from tar sands to provide water substantially reduced in solids content which comprises agitating the sludge with water to provide a diluted sludge with a solids concentration in the range of 6 to 18% by weight, and thereafter settling the sludge to form a lower layer having a solids content substantially higher than that of the sludge an upper layer of bituminous froth, and a middle layer of water having a substantially lower solids content than said undiluted sludge and recovering said upper layer.

REFERENCES:
patent: 3502565 (1970-03-01), Baillie
patent: 3526585 (1970-09-01), Camp
patent: 3931006 (1976-01-01), Baillie et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for reducing mineral content of sludge does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for reducing mineral content of sludge, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for reducing mineral content of sludge will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-101447

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.