ABSTRACT:
A method for reducing the melt fracture during extrusion of a molten narrow molecular weight distribution ethylene polymer which comprises extruding said polymer through a die having a die gap greater than about 50 mils and wherein at least a portion of one surface of the die lip and/or die land in contact with the molten polymer is at an angle of divergence or convergence relative to the axis of flow of the molten polymer through the die.

REFERENCES:
patent: 3376605 (1968-04-01), Beattie
patent: 3382535 (1968-05-01), Ferrari
patent: 3874837 (1975-04-01), Jamieson
patent: 3879507 (1975-04-01), Cavanna
patent: 3914366 (1975-10-01), Wilson
patent: 3920782 (1975-11-01), Cogswell
patent: 3994654 (1976-11-01), Chyu

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for reducing melt fracture during extrusion of ethylene p does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for reducing melt fracture during extrusion of ethylene p, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for reducing melt fracture during extrusion of ethylene p will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2046315

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.