Method for reducing melt fracture during extrusion of a molten n

Plastic and nonmetallic article shaping or treating: processes – Direct application of fluid pressure differential to... – Production of continuous or running length

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

264171, 264173, 264176R, 2642091, 2642097, 2642098, 264216, 4251311, 4251331, 4253261, 425380, 526124, 526128, B29D 2304

Patent

active

043483496

ABSTRACT:
A process for reducing melt fracture formed during extrusion of a molten narrow molecular weight distribution, linear, ethylene polymer, which comprises extruding said polymer through a die having a discharge outlet defining an exit die gap formed by opposing die lip surfaces and wherein one surface of the die lip and/or die land in contact with the molten polymer extends beyond the opposing surface of the die lip and/or die land in the direction of the axis of flow of the molten polymer through the die exit whereby melt fracture is reduced on the surface of the polymer leaving the extended die lip surface.

REFERENCES:
patent: 3023461 (1962-03-01), Sherman
patent: 3574808 (1971-04-01), Matthews et al.
patent: 3784661 (1974-01-01), Schaul et al.
patent: 3876740 (1975-04-01), Egli et al.
patent: 3879158 (1975-04-01), Schele
patent: 3920782 (1975-11-01), Cogswell
patent: 4021170 (1977-05-01), Anderson et al.
patent: 4093692 (1978-06-01), Hill
patent: 4187269 (1980-02-01), Hutchinson et al.
patent: 4203942 (1980-05-01), Sims, Jr. et al.
patent: 4243619 (1981-01-01), Fraser et al.
patent: 4267146 (1981-05-01), Kurtz et al.
patent: 4282177 (1981-08-01), Kurtz et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for reducing melt fracture during extrusion of a molten n does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for reducing melt fracture during extrusion of a molten n, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for reducing melt fracture during extrusion of a molten n will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1341869

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.