Method for reducing caking property of coal

Fuel and related compositions – Liquid fuels – Aluminum or heavy metal – other than lead – containing

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C10L 500

Patent

active

042784425

ABSTRACT:
A method for reducing the caking property of coal, by contacting coal with sulfur dioxide in an amount at least 0.5 times the amount of the coal on a weight basis, at a temperature of at least 120.degree. C. under a pressure of at least 10 Kg/cm.sup.2, and separating the treated coal from the sulfur dioxide, whereby to reduce the caking property of the coal and to render the coal more easily pulverizable.

REFERENCES:
patent: 2336154 (1943-12-01), Wolf
patent: 2739105 (1956-03-01), Ford et al.
patent: 3536589 (1970-10-01), Voet et al.
patent: 3870237 (1975-03-01), Aldrich
patent: 3998604 (1976-12-01), Hinkley
patent: 4018654 (1977-04-01), Johnson et al.
patent: 4120664 (1978-10-01), Gleim
patent: 4169710 (1979-10-01), Jensen
patent: 4198291 (1980-04-01), Yoo et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for reducing caking property of coal does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for reducing caking property of coal, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for reducing caking property of coal will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2162934

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.