ABSTRACT:
Disclosed is a method for recovering acrylic resin from an excess of a sprayed powder coating composition. An excess of the powder coating composition which is not deposited onto an article to be coated and is recovered in a coating apparatus is dissolved in an aromatic hydrocarbon solvent which dissolves the acrylic resin component and which has a solubility of a curing agent of not more than 1.0 g (curing agent)/100 g (solvent) at 20.degree. C. and the acrylic resin component is recovered from the resin solution. The acrylic resin component thus recovered can be reused as a resin component for coating compositions.

REFERENCES:
patent: 3179609 (1965-04-01), Morison
patent: 3714926 (1973-02-01), Ofner
patent: 3737386 (1973-06-01), Geiss et al.
patent: 3975208 (1976-08-01), Tate et al.
patent: 4024815 (1977-05-01), Platsch

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for recovering acrylic resin from excess of sprayed powde does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for recovering acrylic resin from excess of sprayed powde, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for recovering acrylic resin from excess of sprayed powde will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1865560

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.