Method for providing steel with lowered hydrogen level after lad

Specialized metallurgical processes – compositions for use therei – Processes – Producing or treating free metal

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

75305, 106 3827, 164464, 164473, C21C 536

Patent

active

051064120

ABSTRACT:
A method is provided for obtaining steel with lowered hydrogen levels after ladle treatment. The method includes covering molten steel in the ladle with a particulate mixture consisting essentially of calcium aluminate and dolomitic limestone. The mixture is used in amounts of about 5 to 25 pounds per net ton of molten steel. Using the method of this invention, some steels to be cast without vacuum degassing to reduce the hydrogen level.

REFERENCES:
patent: 4373949 (1983-02-01), Spruell et al.
patent: 4417924 (1983-11-01), Schwer
patent: 4795491 (1989-01-01), Quigley
patent: 5028257 (1991-07-01), Tomkins et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for providing steel with lowered hydrogen level after lad does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for providing steel with lowered hydrogen level after lad, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for providing steel with lowered hydrogen level after lad will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1583255

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.