ABSTRACT:
Thermoelectric elements with excellent thermoelectric characteristics such as Seebeck coefficient thermoelectromotive force and thermal conductivity can be produced by molding a powder of metal or metal alloy as the raw material and then sintering; by using as such raw material, ultra fine powders containing Fe and Si as main components and having a mean particle diameter of 50 to 5,000.ANG..

REFERENCES:
patent: 4992235 (1991-02-01), Tokiai et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for producing thermoelectric elements does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for producing thermoelectric elements, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for producing thermoelectric elements will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1695813

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.