Powder metallurgy processes – Powder metallurgy processes with heating or sintering – Powder shape or size characteristics
Patent
1989-03-23
1991-02-12
Lechert, Jr., Stephen J.
Powder metallurgy processes
Powder metallurgy processes with heating or sintering
Powder shape or size characteristics
419 31, 419 38, 419 57, 75 1019, B22F 100
Patent
active
049922351
ABSTRACT:
Thermoelectric elements with excellent thermoelectric characteristics such as Seebeck coefficient thermoelectromotive force and thermal conductivity can be produced by molding a powder of metal or metal alloy as the raw material and then sintering; by using as such raw material, ultra fine powders containing Fe and Si as main components and having a mean particle diameter of 50 to 5,000 .ANG..
REFERENCES:
patent: 4500742 (1985-02-01), Morimoto et al.
patent: 4589918 (1986-05-01), Nishida et al.
patent: 4759905 (1988-07-01), Walter et al.
patent: 4764212 (1988-08-01), Okumura
Tokiai Takeo
Uesugi Takashi
Idemitsu Petrochemical Co. Ltd.
Lechert Jr. Stephen J.
Nigohosian, Jr, Leon
LandOfFree
Method for producing thermoelectric elements does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for producing thermoelectric elements, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for producing thermoelectric elements will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-19381