Coating processes – With stretching or tensioning – Running lengths
Patent
1979-07-24
1980-12-09
Lawrence, Evan K.
Coating processes
With stretching or tensioning
Running lengths
26 96, 427176, 427211, 427290, 427365, 4273982, B05D 312
Patent
active
042385300
ABSTRACT:
A continuous, spliceless bias fabric in which the angular displacement between the warp and filling yarns is in the approximate range of 90 to 150 degrees is produced by the steps of cutting a tubular, square-woven fabric at a bias angle of 40-50 degrees to provide a continuous length of fabric, optionally drying the fabric, calendering at least one layer of an elastomeric compound to at least one side of the continuous length of fabric, heating the thus-calendered fabric, stretching the fabric in its width direction to provide a warp to filling angle of about 90-150 degrees, and cooling the stretched fabric.
REFERENCES:
patent: 1133322 (1915-03-01), Seiberling
patent: 2520699 (1950-08-01), Sowerby et al.
patent: 3784427 (1974-01-01), Griffin
Fieler Wayne C.
Hollaway Gerald C.
Nelson Jack
Spivy Paul L.
Bricker Charles E.
Dayco Corporation
Lawrence Evan K.
Wolk Reuben
LandOfFree
Method for producing stress-relieved fabric does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for producing stress-relieved fabric, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for producing stress-relieved fabric will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2280782