ABSTRACT:
Cured silicone rubber in the form of a finely divided powder is prepared by (1) dispersing a heat-curable liquid silicone rubber composition in water maintained at a temperature of from 0.degree. to 25.degree. C., (2) dispersing the resultant dispersion in a liquid heated to a temperature of at least 50.degree. C., and (3) recovering the resultant cured powder. The liquid silicone rubber composition is preferably maintained at a temperature of from -60.degree. to 0.degree. C. before being emulsified and said liquid is preferably water.
REFERENCES:
patent: 4594134 (1986-06-01), Hanada et al.
Hamada Mitsuo
Shimizu Koji
Yoshida Keiji
Marquis Melvyn I.
Spector Robert
Toray Silicone Co. Ltd.
LandOfFree
Method for producing silicone rubber powder does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method for producing silicone rubber powder, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for producing silicone rubber powder will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1321754