ABSTRACT:
The friability of green needle coke is reduced by heating the green needle coke to a temperature between about 875.degree. F. and about 1,200.degree. F. for a time sufficient to reduce the friability of the green needle coke.

REFERENCES:
patent: 3759795 (1973-09-01), Oliver et al.
patent: 4075084 (1978-02-01), Skripek et al.
patent: 4265710 (1981-05-01), Noguchi et al.
patent: 4521278 (1985-06-01), Kelley et al.
patent: 4545859 (1985-10-01), Kelley et al.
Kou Oil Co. "Production of Calcined Coke With Lower Thermal Expansion Coefficient Under the New Processing Technology", Apr. 29, 1979, 28 pages.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for producing needle coke does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for producing needle coke, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for producing needle coke will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-419492

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.